Product Overview
The 600mm diameter graphite electrode is a high-performance industrial conductive material designed for large electric arc furnaces (EAF) and ladle furnaces (LF). Suitable for high-current-density and high-temperature smelting environments, it offers excellent conductivity, thermal resistance, and mechanical strength, significantly improving smelting efficiency while reducing energy consumption.
Key Features
1,Ultra-High Conductivity
Low resistivity (≤6.0 μΩ·m) ensures efficient current transfer and minimizes power loss.
2,Exceptional Heat Resistance
Withstands instantaneous temperatures up to 2800°C; optional anti-oxidation coating (e.g., aluminum coating) extends service life.
3,High Strength & Fracture Resistance
Flexural strength ≥9 MPa, compressive strength ≥18 MPa, ideal for demanding smelting conditions.
4,Low Thermal Expansion
Coefficient of thermal expansion (CTE) ≤1.8×10⁻⁶/°C (RT to 600°C), ensuring superior thermal stability.
5,Precision-Machined Connections
Standard threading (NPT or ISO) guarantees secure furnace integration and reduces arc loss.


Typical Applications
Steelmaking: EAF steel production, scrap melting, ladle refining.
Non-Ferrous Metals: Silicon, yellow phosphorus, titanium alloy production.
Industrial Silicon/Carbide: Conductive material for submerged arc furnaces.
Other Fields: Monocrystalline silicon growth furnaces, graphitization furnaces.
Technical Specifications
|
Parameter |
Value |
|
Diameter |
600mm (±2mm tolerance) |
|
Length |
Standard 1800-2700mm (customizable) |
|
Bulk Density |
≥1.65 g/cm³ |
|
Resistivity |
≤6.0 μΩ·m |
|
Ash Content |
≤0.7% |
|
Current Capacity |
≥60 kA (operation-dependent) |
Advantages
High-Efficiency Smelting: Optimized for 50-100 ton EAFs, boosting productivity.
Low Consumption: Anti-oxidation design reduces electrode consumption to ≤1.5 kg/ton steel.
Custom Solutions: Supports non-standard lengths, threading, and specialized coatings.
Packaging & Shipping
Moisture-proof wooden crates or steel frames to prevent transit damage.
Store in dry, ventilated areas to avoid humidity exposure.
Usage Guidelines
Preheat to 150-250°C before use to prevent thermal shock cracks.
Regularly inspect electrode joints to ensure stable connections.
Products Parameters
|
Item |
Unit |
RP |
HP |
UHP |
||||
|
≤∅400 |
≥∅450 |
≤∅400 |
≥∅450 |
≤∅400 |
≥∅450 |
|||
|
Electric Resistivity |
Electrode |
μΩ*m |
≤8.5 |
≤9.0 |
≤6.0 |
≤6.5 |
≤5.0 |
≤5.5 |
|
Nipple |
≤6.5 |
≤6.5 |
≤5.5 |
≤5.5 |
≤4.5 |
≤4.5 |
||
|
Transverse Strength |
Electrode |
MPa |
≥8.0 |
≥7.0 |
≥10.5 |
≥10.5 |
≥15.0 |
≥15.0 |
|
Nipple |
≥16.0 |
≥16.0 |
≥20.0 |
≥20.0 |
≥22.0 |
≥22.0 |
||
|
Young's Modulus |
Electrode |
Gpa |
≤9.3 |
≤12.0 |
≤14.0 |
|||
|
Nipple |
≤14.0 |
≤16.0 |
≤18.0 |
|||||
|
Bulk Density |
Electrode |
g/cm3 |
≥1.54 |
≥1.65 |
≥1.68 |
|||
|
Nipple |
≥1.69 |
≥1.73 |
≥1.76 |
|||||
|
Coefficient of Termal Expansion (100℃﹣600℃) |
Electrode |
100-6/℃ |
≤2.5 |
≤2.0 |
≤1.5 |
|||
|
Nipple |
≤2.0 |
≤1.6 |
≤1.2 |
|||||
|
Ash |
% |
≤0.3 |
≤0.2 |
≤0.2 |
||||